Product Description
TEKALOY 90 Percent Tin
Tin - Antimony - Cadmium - Lead Alloy
This pewter is specially formulated for casting flat surfaces that require a high polish. It is suitable for inexpensive jewelry and figurines, where its low melting point lengthens mold life making this alloy ideal for production runs. Sold by the lb.
Casting temperature range: 515-580 °F (268-304 °C)